1500°C Tungsten Carbide Vacuum Sintering Furnace - Cxinduction

1500°C Tungsten Carbide Vacuum Sintering Furnace

Precision sintering for high-performance tungsten carbide (WC) components, with a multi-layer Mo-W hot zone, high-vacuum or inert atmosphere control, and an optional debinding-sintering cycle.

1500°C tungsten carbide vacuum sintering furnace

High-Density WC Sintering

The CXinduction™ 1500°C vacuum sintering furnace is engineered for high-density tungsten carbide (WC) sintering, using a multi-layer molybdenum-tungsten (Mo-W) hot zone for uniform heating and contamination prevention. Designed for powder metallurgy, solid-state sintering and alloy powder processing, it delivers high density in a high-vacuum (≤10⁻³ Pa) or inert gas (Ar/N₂) environment, protecting materials from oxidation.

Need a solution for your project?

Applications of Sintered Tungsten Carbide

Cutting Tools Inserts, end mills and drills — high hardness and wear resistance.
Mining & Construction Wear parts, drill bits and nozzles.
Industrial Components Seals, bearings and valve parts.
Aerospace & Defense High-stress structural components.

Model

CX-SF50/WC Resistance heating; Auto & MAN; 70 kW; usable space 500 × 1000 mm; 196 L loading capacity.

Key Features & Advantages

Multi-Layer Mo/W Hot Zone ±3°C temperature uniformity and shielding against volatile impurities.
High Vacuum & Atmosphere Control Oxygen-free sintering for pure WC and WC-Co alloys.
Debinding-Sintering Integration Vacuum debinding + sintering in one cycle, ideal for binder-jet or MIM parts.
Fast Cooling System Reduces cycle time by 20% versus conventional furnaces.

Technical Parameters

Max Working Temperature 1500°C (1700°C optional)
Temperature Uniformity ±8°C (ΔT between 1000°C and 2200°C)
Heating Rate 1–10°C/min, programmable
Ultimate Vacuum 6.7×10⁻³ mbar (empty, tidy, cold); optional high vacuum 5×10⁻⁵ mbar
Hot Zone Mo + W shielding
Working Atmosphere Fine vacuum; Ar/N₂ inert gas option
Supply Voltage Can be customized
Cooling Water Pressure 2 bar; temperature ≤28°C

Process Considerations

Binder removal: for MIM or pressed parts, heat slowly (1–5°C/min) to 500–600°C to avoid cracking.

Sintering profile: 1400–1500°C for 1–3 hours, varying with grain stabilizers such as Co/Cr.

Related terms: Tungsten carbide vacuum sintering furnace, WC-Co sintering equipment, vacuum debinding sintering furnace, powder metallurgy furnace, solid-state sintering system, alloy powder production furnace, carbide tool manufacturing, MIM sintering furnace, high-vacuum sintering oven, industrial carbide sintering.